Cementing Fluid Loss Additive

Cementing Fluid Loss Additive

*Control fluid loss in normal density cement slurries, lightweight or high density cement slurries.
*Used below temperature of 204.4℃(400℉, BHCT).
*Applicable mixing water: from fresh water to salt-saturated water.
*Compatible well with other additives.
*The product consists of L-type liquid, L-A type anti- freezing liquid, S-P type high purity powder, S-D type dry-mixed powder and S-T type dual-use powder.
Send Inquiry
Description

Tianjin Kelioil Engineering Material and Technology Co., Ltd. is one of the leading manufacturers and suppliers of cementing fluid loss additive in China. Please feel free to buy high quality cementing fluid loss additive at low price from our factory. If you have any enquiry about free sample, please feel free to email us.

 

oilfield cementing additives

When choosing a cementing fluid loss additive, consider multiple factors. Assess the operation environment like formation temperature, pressure, and salt content. In harsh conditions, polymer-based additives with special monomers like 2-acrylamido-2-methylpropane sulfonic acid are suitable. Also, ensure compatibility with the cement system and other admixtures.

Product information

 

PHYSICAL AND CHEMICAL INDICATORS

Type

Appearance

Density, g/cm3

Water-Solubility

CG610L

Colorless or faint yellow liquid

1.10 ± 0.05

Soluble

CG610L-A

Colorless or faint yellow liquid

1.15 ± 0.05

Soluble

 

Type

Appearance

Bulk Density, g/cm3

Water-Solubility

CG610S-P

White or faint yellow powder

0.80±0.20

Soluble

CG610S-D

Grey powder

1.00±0.10

Partly soluble

CG610S-T

White or faint yellow powder

1.00±0.10

Soluble

 

RECOMMENDED DOSAGE

Type

CG610L(-A)

CG610S-P

CG610S-D

CG610S-T

Dosage Range (BWOC)

2.0-8.0%

0.5-2.0%

1.5-5.0%

1.5-5.0%

 

CEMENT SLURRY PERFORMANCE

Item

Test Condition

Technical Indicator

Density of the cement slurry, g/cm3

25℃, Atmospheric Pressure

1.90±0.01

Fluid loss, ml

Fresh water system

80℃, 6.9MPa

≤50

18% salt water system

90℃, 6.9MPa

≤150

Thickening performance

Initial consistency, Bc

80℃/45min, 46.5MPa

≤30

40-100 Bc thickening time, min

≤40

Free fluid, %

80℃, Atmospheric Pressure

≤1.4

24h compressive strength, MPa

≥14

 

 

Select reputable suppliers with rich experience and strict quality control. Choose environmentally friendly additives to reduce ecological impacts. And rely on the supplier's technical support and after-sales service to ensure the smooth progress of cementing operations. At Kelioil, we offer additives that meet all these criteria, providing you with high-quality and reliable solutions for your cementing needs.

oilfield oil well cement fluid loss additive

Product video

 

 

Company profile

factoryteam and office

 

As a professional manufacturer of oilfield additives, Tianjin Kelioil Factory attaches great importance to brand building and market promotion. Through network marketing, participating in international exhibitions and other means, it enhances brand awareness and reputation. Its products are reliable in quality, excellent in performance, and deeply loved by overseas customers. It has established a good brand image in the overseas market.

Certificate

 

oilfield cementing additives certificate

 

Hot Tags: cementing fluid loss additive, China cementing fluid loss additive manufacturers, suppliers, factory, fluid loss requirement, fluid loss benefit strategy, fluid loss price, fluid loss evaluation strategy, fluid loss market strategy, High Temperature Cementing Fluid Loss Additive

Send Inquiry